When the pressure treated film comes off with EFC-38, is it typical to have some fur on the wood? It's happened to me several times with the first wash of a pressure treated deck and it's a pain in the butt. Is my mix too strong? I only use 8oz per five gallons of water and enough pressure to get rid of the PT film.
Lastly, if this is typical, how do you remove the fuzz? I've used a brillo pad once and it seemed to work OK. Sand paper might be better but I'm not sure.
When the pressure treated film comes off with EFC-38, is it typical to have some fur on the wood? It's happened to me several times with the first wash of a pressure treated deck and it's a pain in the butt. Is my mix too strong? I only use 8oz per five gallons of water and enough pressure to get rid of the PT film.
Lastly, if this is typical, how do you remove the fuzz? I've used a brillo pad once and it seemed to work OK. Sand paper might be better but I'm not sure.
Thanks, Nick from Missouri.